Anodizing coating thickness shifted dowel holes on robot end effector mounts
A customer ordered robot end effector mounts with four dowel holes meant to locate a tool plate, and the holes were correct straight off the machine. After anodizing, two holes became too tight, preventing the plate from dropping in. The shop had machined to the blank dimension without accounting for the coating's added thickness inside close-fit bores. The process was changed so dowel holes are finished to the post-anodize size, using masking on some features and slight oversizing on others. The shop notes that coating growth is not perfectly uniform in deep holes, so results still vary on unusual geometries.